Cyclic loading as an extended nanoindentation technique

T. Saraswati, T. Sritharan*, S. Mhaisalkar, C. D. Breach, F. Wulff

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

46 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Cyclic loading as an extended nanoindentation technique'. Together they form a unique fingerprint.

Keyphrases

Material Science