Dive into the research topics of 'Mechanical properties and fractographic analyses of FeCo-2V alloy heat-treated around order-disorder transition temperature'. Together they form a unique fingerprint.- Sort by
- Weight
- Alphabetically
Zhiqiang Li, Vincent Gill, Alexis Lambourne, Zhili Dong, Maxim Avdeev, Joo Tien Oh*, Zhong Chen*
Research output: Contribution to journal › Article › peer-review