Atomic-layer-deposition alumina induced carbon on porous NixCo1-xO nanonets for enhanced pseudocapacitive and Li-ion storage performance

Cao Guan*, Yadong Wang, Margit Zacharias, John Wang, Hong Jin Fan

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

25 Citations (Scopus)

Abstract

A unique composite nanonet of metal oxide@carbon interconnected sheets is obtained by atomic layer deposition (ALD)-assisted fabrication. In this nanonet structure, mesoporous metal oxide nanosheets are covered by a layer of amorphous carbon nanoflakes. Specifically, quasi-vertical aligned and mesoporous NixCo1-xO nanosheets are first fabricated directly on nickel foam substrates by a hydrothermal method. Then, an ALD-enabled carbon coating method is applied for the growth of carbon nanoflakes on the surface of the nanosheets. The thus formed 3D hierarchical structure of NixCo1-xO@carbon composite flakes have a higher surface area, better electrical conductivity and structure stability than the bare NixCo1-xO. The application of such composite nanomaterials is demonstrated as electrodes for a supercapacitor and a lithium-ion battery. In both tests, the composite electrode shows enhancement in capacity and cycling stability. This effective composite nanostructure design of metal oxides@carbon flakes could provide a promising method to construct high-performance materials for energy and environment applications.

Original languageEnglish
Article number014001
JournalNanotechnology
Volume26
Issue number1
DOIs
Publication statusPublished - Jan 9 2015
Externally publishedYes

Bibliographical note

Publisher Copyright:
© 2015 IOP Publishing Ltd.

ASJC Scopus Subject Areas

  • Bioengineering
  • General Chemistry
  • General Materials Science
  • Mechanics of Materials
  • Mechanical Engineering
  • Electrical and Electronic Engineering

Keywords

  • atomic layer deposition
  • carbon
  • energy storage
  • metal oxides

Fingerprint

Dive into the research topics of 'Atomic-layer-deposition alumina induced carbon on porous NixCo1-xO nanonets for enhanced pseudocapacitive and Li-ion storage performance'. Together they form a unique fingerprint.

Cite this