(La0.8Sr0.2)0.9MnO3-Gd 0.2Ce0.8O1.9 composite cathodes prepared from (Gd, Ce)(NO3) x -modified (La0.8Sr 0.2)0.9MnO3 for intermediate-temperature solid oxide fuel cells

Y. J. Leng*, S. H. Chan, K. A. Khor, S. P. Jiang

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

37 Citations (Scopus)

Abstract

Development of high performance cathodes with low polarization resistance is critical to the success of solid oxide fuel cell (SOFC) development and commercialization. In this paper, (La0.8Sr0.2) 0.9MnO3 (LSM)-Gd0.2Ce0.8O 1.9(GDC) composite powder (LSM ~70wt%, GDC ~30 wt%) was prepared through modification of LSM powder by Gd0.2Ce0.8(NO 3) x solution impregnation, followed by calcination. The electrode polarization resistance of the LSM-GDC cathode prepared from the composite powder was ~0.60 Ω cm2 at 750 °C, which is ~13 times lower than that of pure LSM cathode (~8.19 Ω cm2 at 750 °C) on YSZ electrolyte substrates. The electrode polarization resistance of the LSM-GDC composite cathode at 700 °C under 500 mA/cm2 was ~0.42 Ω cm2, which is close to that of pure LSM cathode at 850 °C. Gd0.2Ce0.8(NO3) x solution impregnation modification not only inhibits the growth of LSM grains during sintering but also increases the triple-phase-boundary (TPB) area through introducing ionic conducting phase (Gd,Ce)O2-δ, leading to the significant reduction of electrode polarization resistance of LSM cathode.

Original languageEnglish
Pages (from-to)339-347
Number of pages9
JournalJournal of Solid State Electrochemistry
Volume10
Issue number6
DOIs
Publication statusPublished - Jun 2006
Externally publishedYes

ASJC Scopus Subject Areas

  • General Materials Science
  • Condensed Matter Physics
  • Electrochemistry
  • Electrical and Electronic Engineering

Keywords

  • Composite cathode
  • Impregnation
  • Intermediate-temperature SOFC
  • Polarization resistance

Fingerprint

Dive into the research topics of '(La0.8Sr0.2)0.9MnO3-Gd 0.2Ce0.8O1.9 composite cathodes prepared from (Gd, Ce)(NO3) x -modified (La0.8Sr 0.2)0.9MnO3 for intermediate-temperature solid oxide fuel cells'. Together they form a unique fingerprint.

Cite this