Abstract

We report on the current-carrying capability and the high-current-induced thermal burnout failure modes of 5-20μm diameter double-walled carbon nanotube (DWNT) fibers made by an improved dry-spinning method. It is found that the electrical conductivity and maximum current-carrying capability for these DWNT fibers can reach up to 5.9×10 5Sm -1 and over 1×10 5Acm -2 in air. In comparison, we observed that standard carbon fiber tended to be oxidized and burnt out into cheese-like morphology when the maximum current was reached, while DWNT fiber showed a much slower breakdown behavior due to the gradual burnout in individual nanotubes. The electron microscopy observations further confirmed that the failure process of DWNT fibers occurs at localized positions, and while the individual nanotubes burn they also get aligned due to local high temperature and electrostatic field. In addition a finite element model was constructed to gain better understanding of the failure behavior of DWNT fibers.

Original languageEnglish
Article number015703
JournalNanotechnology
Volume23
Issue number1
DOIs
Publication statusPublished - Jan 13 2012
Externally publishedYes

ASJC Scopus Subject Areas

  • Bioengineering
  • General Chemistry
  • General Materials Science
  • Mechanics of Materials
  • Mechanical Engineering
  • Electrical and Electronic Engineering

Fingerprint

Dive into the research topics of 'Sharp burnout failure observed in high current-carrying double-walled carbon nanotube fibers'. Together they form a unique fingerprint.

Cite this